Cetin, Ali Riza.Hataysal, Ahmet Ercan.Kaplan, Taibe Tokgoz.Botsali, Murat Selim.2020-03-262020-03-262019Cetin, A. R., Hataysal, A. E., Kaplan, T. T., Botsali, M. S. (2019). Depth of Cure and Microhardness of a New Composite vs. Bulk-fill Composites. Journal of Research in Medical and Dental Science, 7(5), 53-59.2347-25452347-2367https://hdl.handle.net/20.500.12395/37654Aim: To compare the depth of cure of new composite with bulk fill resin composites through using Vickers hardness profiles (VHN). Materials and Methods: New composite and four bulk fill composite materials were examined: Tetric N Ceram (R) Bulk Fill, X-tra base, Compon, Filtek Posterior Bulk Fill, Sonic FiIITM. Eight specimens of each material type were prepared in teflon molds which contained a slot of dimensions (8 mm x 4 mm x 2 mm), and a top plate. The molds were irradiated from one end. All specimens were stored at 37 degrees C for 24 h, before measurement. The Vickers hardness was measured as a function of depth of material, at 1 mm intervals. Data were analyzed by one-way ANOVA using Turkey post hoc tests (p=0.05). Results: The maximum VHN ranged from 46.7 to 68.1, whilst the 80% of max. WIN ranged from 374 to 54.5. The depth corresponding to 80% of maximum VHN ranged from 5.5 to 7 mm. This was taken as the depth-of cure. Discussion: In this study, VHN, 80% VHN and depth profile properties of different Bulk Fill resin composites were measured and compared with the new composite by the determination of their VHN/depth profiles. There were statistically significant differences between different bulk fill composite materials in terms of max. VHN and depth of cure, corresponding to 80% of max. VHN. Depth of cure is related to the clinical success of restoration. When a more extensive polymerization and crosslinking occurs,greater VHN results are obtained. According to the manufacturer's claims bulk fill composites can be applied up to 4 mm, or even 5 mm in one time. In general, adequate polymerization along the recommended depth in bulk fill composites is critical to the long-term stability of restorations. According to the results of our research, the manufacturers' claim was approved for these materials. Conclusion: New composite can be cured to an acceptable post-cure depth as Bulk fill resin composites, according to the manufacturers' claims. X-tra base had the greatest depth of cure among the composites examined.eninfo:eu-repo/semantics/openAccessBulk fill compositesMicrohardnessDepth of cureDepth of cure and microhardness of a new composite vs. bulk-fill compositesArticle755359#YOKWOS:000497956500010N/A