Synthesis and Properties of Boron Doped NaxCo2O4 Nanocrystalline Ceramics

dc.contributor.authorUslu, I.
dc.contributor.authorCetin, Saime Sebnem
dc.contributor.authorAytimur, A.
dc.contributor.authorYuceyurt, S.
dc.contributor.authorErdal, M. O.
dc.date.accessioned2020-03-26T18:31:29Z
dc.date.available2020-03-26T18:31:29Z
dc.date.issued2012
dc.departmentSelçuk Üniversitesien_US
dc.description.abstractSodium cobalt oxide (NaCo2O4) nanofibers with diameters ranging between 20 and 200 nm were prepared by electrospinning a precursor mixture of PVA/(Na-Co) acetate. This was the first time any such attempt was made. Afterwards, the electrospun nanofibers were subjected to calcination treatment. The characteristics of the fibers were investigated using a Fourier transform infrared spectroscopy, a X-ray diffractometer, and a scanning electron microscopy. The boron doped and undoped NaCo2O4 nanofibers calcined at 850 A degrees C were polycrystalline of the gamma NaxCo2O4 phase having diameters ranging between 20 and 60 nm with grain sizes of 5-10 nm, and the nanofibers calcined at 800 A degrees C were single crystals having linked particles or crystallites with particle sizes ranging between 60 and 200 nm. The results indicated a significant effect of calcination temperature on the crystalline phase and morphology of the nanofibers. It could be seen in the SEM micrograph of the fibers that when boron was added, this resulted in the formation of cross-linked bright-surfaced fibers. The average fiber diameter for boron doped and undoped fiber mats were 204 and 123 nm, respectively. The grain diameters of boron doped and undoped nanocrystalline sintered powders were measured as 140 and 118 nm, respectively.en_US
dc.identifier.doi10.1007/s10904-011-9644-xen_US
dc.identifier.endpage771en_US
dc.identifier.issn1574-1443en_US
dc.identifier.issn1574-1451en_US
dc.identifier.issue4en_US
dc.identifier.scopusqualityQ2en_US
dc.identifier.startpage766en_US
dc.identifier.urihttps://dx.doi.org/10.1007/s10904-011-9644-x
dc.identifier.urihttps://hdl.handle.net/20.500.12395/28455
dc.identifier.volume22en_US
dc.identifier.wosWOS:000305224400012en_US
dc.identifier.wosqualityQ3en_US
dc.indekslendigikaynakWeb of Scienceen_US
dc.indekslendigikaynakScopusen_US
dc.language.isoenen_US
dc.publisherSPRINGERen_US
dc.relation.ispartofJOURNAL OF INORGANIC AND ORGANOMETALLIC POLYMERS AND MATERIALSen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.selcuk20240510_oaigen_US
dc.subjectElectrospinningen_US
dc.subjectSodium cobalt oxideen_US
dc.subjectNanofibersen_US
dc.subjectNa-Co acetateen_US
dc.subjectPoly (vinyl) alcoholen_US
dc.titleSynthesis and Properties of Boron Doped NaxCo2O4 Nanocrystalline Ceramicsen_US
dc.typeArticleen_US

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
28455.pdf
Boyut:
589.25 KB
Biçim:
Adobe Portable Document Format
Açıklama:
Makale Dosyası