Strength of Filament Wound GRP Pipes with Surface Crack

dc.contributor.authorTarakçıoğlu, Necmettin
dc.contributor.authorAkdemir, Ahmet
dc.contributor.authorAvcı, Ahmet
dc.date.accessioned2020-03-26T16:37:24Z
dc.date.available2020-03-26T16:37:24Z
dc.date.issued2001
dc.departmentSelçuk Üniversitesien_US
dc.description.abstractIn this work, the effect of surface cracks on strength has been investigated theoretically and experimentally for glass/epoxy filament wound pipes, which are mainly used for bazooka launchers. The pipes with surface crack which have several notch-aspect ratios ale and notch-to-thickness ratios a/t in the axial direction were exposed to open-ended internal pressure. Critical stress intensity factors were determined experimentally for several winding angles by tensile tests with center notched ring specimens. The strength values of pipes with surface cracks are compared with internal pressure test results and theoretical results.en_US
dc.identifier.citationTarakçıoğlu, N., Akdemir, A., Avcı, A., (2001). Strength of Filament Wound GRP Pipes with Surface Crack. Composites Part B-Engineering, 32(2), 131-138. Doi:10.1016/S1359-8368(00)00037-8
dc.identifier.doi10.1016/S1359-8368(00)00037-8en_US
dc.identifier.endpage138en_US
dc.identifier.issn1359-8368en_US
dc.identifier.issn1879-1069en_US
dc.identifier.issue2en_US
dc.identifier.scopusqualityQ1en_US
dc.identifier.startpage131en_US
dc.identifier.urihttps://dx.doi.org/10.1016/S1359-8368(00)00037-8
dc.identifier.urihttps://hdl.handle.net/20.500.12395/17613
dc.identifier.volume32en_US
dc.identifier.wosWOS:000167418100005en_US
dc.identifier.wosqualityQ1en_US
dc.indekslendigikaynakWeb of Scienceen_US
dc.indekslendigikaynakScopusen_US
dc.language.isoenen_US
dc.publisherELSEVIER SCI LTDen_US
dc.relation.ispartofComposites Part B-Engineeringen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.selcuk20240510_oaigen_US
dc.subjectpolymer-matrix composites (PMCs)en_US
dc.subjectstrengthen_US
dc.subjectfilament windingen_US
dc.subjectsurface cracken_US
dc.titleStrength of Filament Wound GRP Pipes with Surface Cracken_US
dc.typeArticleen_US

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
40bad05fde456e1c757caa436d23ba7e.pdf
Boyut:
619.93 KB
Biçim:
Adobe Portable Document Format
Açıklama: