Surface roughness and hardness of some dental ceramics and restorative resins

Yükleniyor...
Küçük Resim

Tarih

2004

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

TRANS TECH PUBLICATIONS LTD

Erişim Hakkı

info:eu-repo/semantics/openAccess

Özet

The aim of this study was to compare the surface hardness and roughness of seven composite resins AElite LS(AE), Clearfil Poto Posterior(CPP), SureFil (SF), Tetric Ceram (TC), Artglass (AG), Admira (AD), Estenia (ES)) and two ceramic materials (Vitadur Alfa (VA), Finesse(FI)). The composite speciemens were cured in cylindirical brass molds (4mm, in diameter and 2 mm in depth) against glass according to manufacturers' directions and polished. The ceramic specimens were prepared in same diameters, glazed. Hardness was determined at two different sites on one side specimens and the mean value was calculated as Vicker's Hardness Numbers (VHN). Surface roughness (SR) was measured tree times as Ra (mum) on each specimen and mean roughness values were obtained. For statistical analyses Mann Whitney U test was used. Surface roughness values of CPP, ES were very close to that of VA. Their surface roughness values were significantly higher than other materials. VHN of ES and AG were significantly lower than that of two ceramic materials. The surface hardness of ES was significantly harder than composite resins (P<0.05)

Açıklama

8th Conference of the European-Ceramic-Society -- JUN 29-JUL 03, 2003 -- Istanbul, TURKEY

Anahtar Kelimeler

hardness, roughness, composite resin and ceramic