Failure Analysis of (+/- 55 Degrees)(3) Filament Wound Composite Pipes With an Inclined Surface Crack Under Static Internal Pressure

Yükleniyor...
Küçük Resim

Tarih

2010

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

Elsevier Sci Ltd

Erişim Hakkı

info:eu-repo/semantics/openAccess

Özet

This study conducts failure analysis of filament wound glass reinforced plastic (GRP) pipes made of E-glass/epoxy with an inclined surface crack under open-ended internal pressure. Test specimens are composed of six antisymmetric layers with (+/- 55 degrees)(3) winding angles. Tests have been performed at seven different crack angles: 0 degrees, 15 degrees, 30 degrees, 60 degrees, 45 degrees, 75 degrees, and 90 degrees, with crack-to-thickness ratio of a/t = 0.50. The burst strengths of the specimens were determined, and the dependence of the burst strength on the crack angle was examined.

Açıklama

Anahtar Kelimeler

GRP pipe, Inclined surface crack, Burst strength, Internal pressure

Kaynak

Composite Structures

WoS Q Değeri

Q1

Scopus Q Değeri

Q1

Cilt

92

Sayı

Künye

Arıkan, H., (2010). Failure Analysis of (+/- 55 Degrees)(3) Filament Wound Composite Pipes With an Inclined Surface Crack Under Static Internal Pressure. Composite Structures, (92), 182-187. Doi: 10.1016/j.compstruct.2009.07.027