dc.description.abstract | The purpose of this study was to investigate the dentin bond durability of a one-step, fluoride-containing, glass ionomer-based adhesive system, Reactmer Bond (RB), and that of a two-step, fluoride-containing, self-etch adhesive system, Clearfil Protect Bond (CPB). Enamel was removed from the occlusal surfaces of teeth, and flat dentin surfaces were entirely covered with a composite resin following the application of an adhesive material (n=10). After specimens were sectioned into rectangular sticks of 0.87 +/- 0.03 mm(2), the sticks were randomly assigned into two accelerated aging time period groups: 1 week or 1 year. Microtensile bond strengths were determined. Bond strength of RB increased significantly after 1 year (1 week=27.80 +/- 10.57 MPa versus 1 year=36.93 +/- 14.38 MPa) (p<0.05). In contrast, there was no significant difference in bond strength between the two time periods for CPB (1 week=51.74 +/- 17.8 MPa versus 1 year=56.03 +/- 18.85 MPa) (p>0.05). Both fluoride-containing adhesives seemed to demonstrate reliable bonding performance after 1 year of accelerated aging in water. | en_US |
dc.identifier.doi | 10.4012/dmj.2013-107 | en_US |
dc.identifier.endpage | 97 | en_US |
dc.identifier.issn | 0287-4547 | en_US |
dc.identifier.issue | 1 | en_US |
dc.identifier.pmid | 24492118 | en_US |
dc.identifier.scopusquality | Q1 | en_US |
dc.identifier.startpage | 92 | en_US |
dc.identifier.uri | https://dx.doi.org/10.4012/dmj.2013-107 | |
dc.identifier.uri | https://hdl.handle.net/20.500.12395/30760 | |
dc.identifier.volume | 33 | en_US |
dc.identifier.wos | WOS:000333442400015 | en_US |
dc.identifier.wosquality | Q3 | en_US |
dc.indekslendigikaynak | Web of Science | en_US |
dc.indekslendigikaynak | Scopus | en_US |
dc.indekslendigikaynak | PubMed | en_US |
dc.language.iso | en | en_US |
dc.publisher | JAPANESE SOC DENTAL MATERIALS DEVICES | en_US |
dc.relation.ispartof | DENTAL MATERIALS JOURNAL | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.selcuk | 20240510_oaig | en_US |
dc.subject | Adhesion | en_US |
dc.subject | Bond durability | en_US |
dc.subject | Glass ionomer adhesive | en_US |
dc.subject | Microtensile bond strength | en_US |
dc.subject | Self-etch adhesive | en_US |
dc.title | Effect of accelerated aging on the bonding performance of fluoridated adhesive resins | en_US |
dc.type | Article | en_US |